+86 0769 82915639

Home > PRODUCT > Cement industry Wear-Resistant welding wire

RD-138 (6686在线)

Cement grinding rolls, grinding discs, extrusion rolls, crusher rotors priming/transition layer surfacing

Consultation:

Email: echo_rongda@bjzxjt.cn

WhatsApp: +86 13929460585

Product details:

RD-138

——————————————————————————————————————————————

Cement grinding rolls, grinding discs, extrusion rolls, crusher rotors priming/transition layer surfacing


Material Characteristics
The post-weld material is an extremely tough, crack-resistant cladding material with high extrusion stress, austenitic in nature, and characterized by hardening (work hardening) when impacted.
1.Microstructure: Austenitic chromium-manganese steel;Alloy Type:C-Cr-Mn-Fe2.Processing performance: only support sanding     
3.Cutting performance: does not support flame cutting4.Surfacing thickness: supports multi-layer surfacing


Applications
Typically used as an overlay transition and priming layer to facilitate overlaying of harder overlay materials: e.g. transition/priming layer for overlaying of grinding rolls, grinding discs, extrusion rolls, crusher rotors; also used in the manufacture or repair of crane wheels, rope pulleys, wire-drawing discs, etc...


Main chemical composition of pure welding layer
C CrMnSiP S Ni MoNb WOthers
0.1-0.2%9.0-15.0%15-20%0.5-1.0%≤0.04%
≤0.04%0.2-0.8%///≤1.0%
Hardness of pure welding layer                                                          Packaging specification
HRC 20-40                                   

125/150/250  KG/Barrel

Recommended Surfacing Parameters
Wire Diameter      Current     Voltage  Wire Stick-out Length
2.4/2.8/3.2mm     250-430A     27-32V25-40mm


Welding Precautions

1 6686平台. When using RD-138 welding wire, do not use inert gas, and pay attention to control the current and voltage according to the recommended surfacing parameters.

2 6686手机版. Oscillating and straight line welding can be, can be overlaid with multiple layers, the performance of the alloy layer and the dilution rate of the overlaid welding.

3 6686注册. Each layer of weld should be cleaned up after welding slag before welding the next layer, and so on.


1.png

2.png

3.png

4.png